Why does a screed crack and what can be done?

Usually because of drying that was too fast or missing joints. Before repairing, you need to establish whether the crack is stabilised or still active.

A crack isn't necessarily serious, but it should never be ignored. The first step isn't to fill it, but to identify it. Surface crazing and an active, widening crack require completely different treatments.

‍

The three types of cracks

Thecrazing forms a network of fine, superficial, spiderweb-like cracks. It is caused by the surface drying too quickly. It poses no structural risk and does not prevent the installation of tiles, but it must be treated before laying flexible flooring.

Thethrough-crack is straight and runs all the way through the material. It is generally caused by restrained shrinkage: missing joints, an area that is too large, or a screed blocked against a wall due to a lack of perimeter strip.

Theactive crack continues to widen over time. The cause is not in the screed itself but underneath it: a moving slab, a flexing floor, or settlement. Treating it without addressing the underlying cause is pointless.

‍

The most common causes

  • Drying too quickly in the first few days due to drafts, direct sunlight, or forced-air heating.
  • Absence or excessive spacing of control joints.
  • Excess mixing water, which significantly increases shrinkage.
  • Insufficient thickness for the type of screed and substrate.
  • Lack of mesh on a compressible or deformable substrate.
  • Starting a heated floor too early or too abruptly.

‍

Stable or active: the essential test to perform first

Place a plaster or glass tell-tale across the crack and date it. Monitor it for two to four weeks. If it breaks, the crack is still active, and a structural assessment is required before any repairs. If it remains intact, the crack is stable and can be treated.

‍

How to repair a stable crack

The principle is to stitch the screed back together, not just cover up the crack. We open the crack into a V-shape, carefully remove all dust, and then inject it with epoxy resin. Metal staples are inserted perpendicular to the crack into grooves spaced 20 to 30 cm apart, followed by a finishing leveling compound.

Simply filling it with mortar will cause it to reopen with the first change in temperature. And the best repair is the one you never have to make: mistakes to avoid before pouring a screed prevent most of these issues.

Most recent questions

During the works
Insulation
Underfloor heating

Can underfloor heating be laid directly on the insulation?

Yes, that is the rule: the pipes are fixed on the insulation layer, then embedded in the screed. The insulation must be flat, resist compression and be covered with a membrane.

Before the works
Insulation
Renovation

Should you insulate an upper floor above a heated room?

Thermally, hardly: heat does not leak between two heated rooms. Upstairs, acoustic insulation against impact noise is what matters, except above an unheated space.

During the works
Insulation

How long between sprayed PUR and the screed?

Sprayed PUR sets in under 24 hours. The screed can follow as soon as the foam is sanded level and covered with a membrane, often within a few days depending on the site schedule.

Before the works
Insulation

Is sprayed PUR affected by moisture in the base?

Once in place, closed-cell PUR absorbs little water. But it must be sprayed onto a dry base, and it does not replace treating moisture rising from the ground.

Need a reliable partner for solid screeds, or thermal or acoustic insulation?

Contact us
Arrow right icon